Xylan Coating Statistic
Tensile Strength (ASTM D1708)4000 - 5000 psi
Elongation (ASTM D1457)50%
Impact Strength (ASTM D256)13 ft - lb/in
Hardness (ASTM D2240)60 - 90 HB (Shore D)
Abrasion Resistance (Tabor)>15 mg
Coefficient of Friction (ASTM D1894)0.15 - 0.35 static
Dielectric Strength (ASTM D149)1400 volts per mil
Use Temperature-100 Degree F to 500 Degree F max
Melting Pointn/a
Thermal Conductivityn/a
Chemical Resistance (ASTM D543)Good
Salt Spray Resistance (ASTM B117)Excellent
Water Absorption (ASTM D570)<0.03 %
Thickness0.0008” - 0.002 ”